Repository logo
  • English
  • Català
  • Čeština
  • Deutsch
  • Español
  • Français
  • Gàidhlig
  • Italiano
  • Latviešu
  • Magyar
  • Nederlands
  • Polski
  • Português
  • Português do Brasil
  • Suomi
  • Svenska
  • Türkçe
  • Қазақ
  • বাংলা
  • हिंदी
  • Ελληνικά
  • Yкраї́нська
  • Log In
    or
    New user? Click here to register.Have you forgotten your password?
Repository logo
  • Communities & Collections
  • Research Outputs
  • Fundings & Projects
  • People
  • Statistics
  • English
  • Català
  • Čeština
  • Deutsch
  • Español
  • Français
  • Gàidhlig
  • Italiano
  • Latviešu
  • Magyar
  • Nederlands
  • Polski
  • Português
  • Português do Brasil
  • Suomi
  • Svenska
  • Türkçe
  • Қазақ
  • বাংলা
  • हिंदी
  • Ελληνικά
  • Yкраї́нська
  • Log In
    or
    New user? Click here to register.Have you forgotten your password?
  1. Home
  2. Indian Institute of Technology Madras
  3. Publication9
  4. Mechanical and wear behaviour of alloyed hypereutectic grey cast iron
 
  • Details
Options

Mechanical and wear behaviour of alloyed hypereutectic grey cast iron

Date Issued
01-07-2010
Author(s)
Vadiraj, A.
Balachandran, G.
Kamaraj M 
Indian Institute of Technology, Madras
Gopalakrishna, B.
Rao, D. V.
DOI
10.1179/026708309X12454008169429
Abstract
Alloyed grey cast iron is an important automotive material used in clutch and brake applications. In order to understand the influence of microalloying additives on the graphitic morphology, mechanical and wear behaviour, a series of microalloyed cast iron melts were taken. The laboratory scale ingots made were characterised for microstructure, mechanical properties and wear behaviour. All the cast irons made were hypereutectic with a microstructure consisting of class A type graphite in a pearlitic matrix with eutectic grain boundary carbides. The microalloyed cast irons showed two- to threefold improved wear resistance over a base unalloyed material at comparable mechanical strengths. The wear loss was found to be linear with increasing sliding distance, and the wear resistance is attributed to the combined influence of dense pearlitic matrix with carbides and good distribution of graphite flakes. Cast iron microalloyed with Ni (0.62%) with Ce inoculation showed best overall properties compared to other alloys. © 2010 Maney Publishing.
Volume
26
Subjects
  • Alloyed grey cast iro...

  • Microstructure

  • Wear

Indian Institute of Technology Madras Knowledge Repository developed and maintained by the Library

Built with DSpace-CRIS software - Extension maintained and optimized by 4Science

  • Cookie settings
  • Privacy policy
  • End User Agreement
  • Send Feedback