A two-step method for synthesis of micron sized nanoporous silver powder and ZnO nanoparticles
Date Issued
01-10-2017
Author(s)
Bhushan, B.
Murty, B. S.
Mondal, K.
Abstract
Micron-sized nanoporous silver powder with pore size of ∼100–160 nm and specific surface area of ∼4.7–5.5 m2/g was synthesized from three mechanically alloyed Ag-Zn powders (composition: 25, 50 and 75 at.% Zn). Dealloying was carried out at free corrosion conditions in NaOH, HCl and AgNO3 solutions. Both partial and complete dealloying were obtained by suitable choice of electrolyte and time of exposure. Zn in the solution after dealloying was recovered in the form of ZnO nanoparticles with particle size of 55.7 ± 18 nm. The effect of composition and electrolyte on the degree of dealloying was also studied.
Volume