Options
Catalytic decomposition of N<inf>2</inf>O on La<inf>2</inf>CuO<inf>4</inf> in the presence of LaNi<inf>5</inf> alloy
Date Issued
01-03-1989
Author(s)
Christopher, J.
Swamy, C. S.
Abstract
Decomposition of N2O has been studied on pure La2CuO4, La2CuO4 with 5 and 10 wt. % LaNi5 and oxidized LaNi5 in the temperature range of 240-490 °C at 50 and 200 Torr initial pressures of N2O. The addition of LaNi5 decreases the energy of activation compared to that of La2CuO4 which has been explained based on the dispersity of NiO over La2CuO4. © 1989 Akadémiai Kiadó.
Volume
39